CytoSoft Q&A

Q1: Why should the CytoSoft surfaces not be allowed to dry? A1: 0.2, 0.5 and 2 kPa silicone gel can crack if their surface is allowed to dry. Q2: Are the CytoSoft plates reusable? A2: Cell matrix proteins are attached to the surface of the gel via covalent bonding. It is difficult to form a […]

Read More

Tropoelastin Information Q&A

Tropoelastin Information Q&A 9-4-2017

Read More

Concentration of Silk Fibroin

Q: How is the concentration of Silk Fibroin determined? A: We use the dry down method. (Weigh out a certain amount of silk fibroin and leave in a 60C oven overnight, and weigh the left-over protein).

Read More

Donor Consent for Type III and Type IV Human Collagen Products

Donor Consent for Type III and Type IV Human Collagen Products

Read More

Purity of PureCol Collagen 99.9%

Purity of PureCol collagen (Vitrogen)

Read More